FAQ · Installation & Training

Laser Spot Welder Parameter Setup: Energy, Pulse Width and Focus

Updated Nov 26, 2026 Installation & Training

Setting up a laser spot welder is easier when you follow a fixed sequence and verify each change with a test coupon.

Step 1: Energy

Start from a low energy setting and increase gradually until the weld penetrates correctly. Too little energy causes weak welds; too much causes burn-through.

Step 2: Pulse Width

Longer pulse width adds more heat. Use a shorter pulse for fine work and a longer pulse where more penetration is needed.

Step 3: Focus

Check the focus position and focus offset. A correct focus gives a stable spot; an incorrect one reduces energy density and consistency.

Verify With Test Coupons

Test on the same material and thickness as production. Inspect the spot for penetration, splatter and surface damage before starting the batch.

Need help? Ask an engineer

Share material, thickness and requirements. We will suggest a process.

Get a
Quote
Call Us WhatsApp